header

Bond degradation resistance of nano - bond adhesive system bonded to dentin : (Record no. 50849)

MARC details
000 -LEADER
fixed length control field 02130cam a2200313 a 4500
003 - CONTROL NUMBER IDENTIFIER
control field EG-GiCUC
008 - FIXED-LENGTH DATA ELEMENTS--GENERAL INFORMATION
fixed length control field 150509s2011 ua o f m 000 0 eng d
040 ## - CATALOGING SOURCE
Original cataloging agency EG-GiCUC
Language of cataloging eng
Transcribing agency EG-GiCUC
041 0# - LANGUAGE CODE
Language code of text/sound track or separate title eng
049 ## - LOCAL HOLDINGS (OCLC)
Holding library Deposite
097 ## - Thesis Degree
Thesis Level M.Sc
099 ## - LOCAL FREE-TEXT CALL NUMBER (OCLC)
Classification number Cai01.09.03.M.Sc.2011.Ta.B
100 0# - MAIN ENTRY--PERSONAL NAME
Personal name Tamer Zui Hemma
245 10 - TITLE STATEMENT
Title Bond degradation resistance of nano - bond adhesive system bonded to dentin :
Remainder of title In vivo study /
Statement of responsibility, etc. Tamer Zui Hemma ; Supervised Mona Ismail Riad , Sahar Ahmed Abdelhalim
246 15 - VARYING FORM OF TITLE
Title proper/short title مقاومة تدهور الربط لنظام اللصق النانو مترى إلى العاج السنى :
Remainder of title دراسة حية
260 ## - PUBLICATION, DISTRIBUTION, ETC.
Place of publication, distribution, etc. Cairo :
Name of publisher, distributor, etc. Tamer Zui Hemma ,
Date of publication, distribution, etc. 2011
300 ## - PHYSICAL DESCRIPTION
Extent 103 Leaves :
Other physical details photographs ;
Dimensions 30cm
502 ## - DISSERTATION NOTE
Dissertation note Thesis (M.Sc.) - Cairo University - Faculty of Oral and Dental Medicine - Department of Opertive Dentistry
520 ## - SUMMARY, ETC.
Summary, etc. This study was carried to evaluate the invivo bond degradation resistance of light and dual cure Nano Bond adhesive system by assessing the nanoleakage of class II resin composite restoration with and without etching, and interfacial analysis using ESEM and to investigate whether the curing mode and pre - etching could affect microtensile bond strength at 24 hours and after 3 monthes. Standardized class II cavities were prepared in 80 premolars of 20 patients. Dual and light cured Nano bond self etch adhesive was applied with and without pre - treatment. Then, teeth were extracted as part of orthodontic treatment according to testing periods. Sticks of 1mm2 cross section were prepared for testing both microtensile bond strength and nanoleakage evaluation. The results were presented as mean and SD values; repeated measures anova followed by Mann - whitney test were used to analyze the results
530 ## - ADDITIONAL PHYSICAL FORM AVAILABLE NOTE
Additional physical form available note Issued also as CD
653 #4 - INDEX TERM--UNCONTROLLED
Uncontrolled term Bond degradation resistance
653 #4 - INDEX TERM--UNCONTROLLED
Uncontrolled term Dentin
653 #4 - INDEX TERM--UNCONTROLLED
Uncontrolled term Nano - bond adhesive system bonded
700 0# - ADDED ENTRY--PERSONAL NAME
Personal name Mona Ismail Riad ,
Relator term
700 0# - ADDED ENTRY--PERSONAL NAME
Personal name Sahar Ahmed Abdelhalim ,
Relator term
905 ## - LOCAL DATA ELEMENT E, LDE (RLIN)
Cataloger Nazla
Reviser Revisor
905 ## - LOCAL DATA ELEMENT E, LDE (RLIN)
Cataloger Samia
Reviser Cataloger
942 ## - ADDED ENTRY ELEMENTS (KOHA)
Source of classification or shelving scheme Dewey Decimal Classification
Koha item type Thesis
Holdings
Source of classification or shelving scheme Not for loan Home library Current library Date acquired Full call number Barcode Date last seen Koha item type Copy number
Dewey Decimal Classification   المكتبة المركزبة الجديدة - جامعة القاهرة قاعة الرسائل الجامعية - الدور الاول 11.02.2024 Cai01.09.03.M.Sc.2011.Ta.B 01010110065541000 22.09.2023 Thesis  
Dewey Decimal Classification   المكتبة المركزبة الجديدة - جامعة القاهرة مخـــزن الرســائل الجـــامعية - البدروم 11.02.2024 Cai01.09.03.M.Sc.2011.Ta.B 01020110065541000 22.09.2023 CD - Rom 65541.CD