The effect of finishing technique on the surface roughness and fracture resistance of In ceram crowns / (Record no. 56102)

MARC details
000 -LEADER
fixed length control field 03332cam a2200337 a 4500
003 - CONTROL NUMBER IDENTIFIER
control field EG-GiCUC
005 - DATE AND TIME OF LATEST TRANSACTION
control field 20250223031457.0
008 - FIXED-LENGTH DATA ELEMENTS--GENERAL INFORMATION
fixed length control field 160420s2014 ua dh f m 000 0 eng d
040 ## - CATALOGING SOURCE
Original cataloging agency EG-GiCUC
Language of cataloging eng
Transcribing agency EG-GiCUC
041 0# - LANGUAGE CODE
Language code of text/sound track or separate title eng
049 ## - LOCAL HOLDINGS (OCLC)
Holding library Deposite
097 ## - Thesis Degree
Thesis Level M.Sc
099 ## - LOCAL FREE-TEXT CALL NUMBER (OCLC)
Classification number Cai01.09.09.M.Sc.2014.Mo.E
100 0# - MAIN ENTRY--PERSONAL NAME
Personal name Mohammed Alaa Alsibai
245 14 - TITLE STATEMENT
Title The effect of finishing technique on the surface roughness and fracture resistance of In ceram crowns /
Statement of responsibility, etc. Mohammed Alaa Alsibai ; Supervised Jylan Alguindy , Zeinab Nabil
246 15 - VARYING FORM OF TITLE
Title proper/short title تأثرطرق الانھاء على مقاومه الكسرفي التيجان الخزفيه
260 ## - PUBLICATION, DISTRIBUTION, ETC.
Place of publication, distribution, etc. Cairo :
Name of publisher, distributor, etc. Mohammed Alaa Alsibai ,
Date of publication, distribution, etc. 2014
300 ## - PHYSICAL DESCRIPTION
Extent 123 P. :
Other physical details charts , facsimiles ;
Dimensions 25cm
502 ## - DISSERTATION NOTE
Dissertation note Thesis (M.Sc.) - Cairo University - Faculty of Oral and Dental Medicine- Department of Prosthodontics
520 ## - SUMMARY, ETC.
Summary, etc. The aim of this present study was to investigate the effect of different finishing techniques (A: Glazing, B: Re-glazing, C: polishing) on the fracture resistance and surface roughness of In - Ceram crowns. A total of thirty coping core samples were constructed by using (CAD/CAM system) and divided into two equal groups(15 for each groups) group A: In ceram zirconia blocks and group B: In ceram Alumina blocks, all samples then veneered by veneering material accordingto manufacture instruction. Each group were further subdivided according to the type of finishing technique into three equal subgroups (n = 5): subgroup I (A): autoglazed samples (control group), subgroup II (G): re- glazed samples after surface adjustment and subgroup III (P): polished samples using the recommended polishing kitby the manufacturer. The crowns shaped samples were cemented on epoxy - resin dies and where subject to fracture load testing using universal testing machine. Scanning electron microscopy (SEM) was employed to examine the morphology of the ceramic surface after different finishing techniques. Data were collected and statistically analyzed. For In ceram zirconiacrowns the results showed the polishing technique had significanthighest mean load at failure than other techniques, whilefor In ceram Alumina crownsexhibited a significantly higher mean load at failure with the glazing procedures.The results also revealedthe In ceram zirconia crowns had significantly highest mean of surface roughness for re- glazing and glazing techniques, while the polishing technique showed the statistically significant highest mean of surface roughness for In ceram Alumina crowns. Finishing and polishing of In-ceram zirconia crowns results higher fracture resistance than that produced with the glazing and re-glazing procedures. In-ceram alumina crowns exhibited a significantly higher fracture resistance with the glazing procedures. Glazing and re- glazing for In-ceram zirconia crowns results in more rougher surfaces than that with finishing and polishing procedures
530 ## - ADDITIONAL PHYSICAL FORM AVAILABLE NOTE
Additional physical form available note Issued also as CD
653 #4 - INDEX TERM--UNCONTROLLED
Uncontrolled term In ceram aluminafracture resistance
653 #4 - INDEX TERM--UNCONTROLLED
Uncontrolled term In ceram zirconia
653 #4 - INDEX TERM--UNCONTROLLED
Uncontrolled term Surface roughness
700 0# - ADDED ENTRY--PERSONAL NAME
Personal name Jylan Alguindy ,
Relator term
700 0# - ADDED ENTRY--PERSONAL NAME
Personal name Zeinab Nabil,
Relator term
856 ## - ELECTRONIC LOCATION AND ACCESS
Uniform Resource Identifier <a href="http://172.23.153.220/th.pdf">http://172.23.153.220/th.pdf</a>
905 ## - LOCAL DATA ELEMENT E, LDE (RLIN)
Cataloger Aml
Reviser Cataloger
905 ## - LOCAL DATA ELEMENT E, LDE (RLIN)
Cataloger Nazla
Reviser Revisor
942 ## - ADDED ENTRY ELEMENTS (KOHA)
Source of classification or shelving scheme Dewey Decimal Classification
Koha item type Thesis
Holdings
Source of classification or shelving scheme Not for loan Home library Current library Date acquired Full call number Barcode Date last seen Koha item type Copy number
Dewey Decimal Classification   المكتبة المركزبة الجديدة - جامعة القاهرة قاعة الرسائل الجامعية - الدور الاول 11.02.2024 Cai01.09.09.M.Sc.2014.Mo.E 01010110068645000 22.09.2023 Thesis  
Dewey Decimal Classification   المكتبة المركزبة الجديدة - جامعة القاهرة مخـــزن الرســائل الجـــامعية - البدروم 11.02.2024 Cai01.09.09.M.Sc.2014.Mo.E 01020110068645000 22.09.2023 CD - Rom 68645.CD