header
Local cover image
Local cover image
Image from OpenLibrary

Evaluation of marginal integrity of lithium disilicate vonlays versus celtra duo vonlays restoring premolars : (in vitro study) / Hozaifa Abd ElBaset Elnaggar ; supervisors Prof. Dr. Lamia Khairallah, Dr.Noha Adel El Khodary, Dr. Abu Bakr Hashem.

By: Contributor(s): Material type: TextTextLanguage: English Summary language: English, Arabic Producer: 2021Description: vi, 83 pages : color illustrations ; 25 cm. + CDContent type:
  • text
Media type:
  • Unmediated
Carrier type:
  • volume
Other title:
  • دقة الحواف للضواحك المرممة بالقشور السطحية الخزفية المصنعة من الليثيوم دايسيليكات بالمقارنة مع القشور السطحية الخزفية المصنعة من السيلترا ديو : دراسة معملية [Added title page title]
Subject(s): DDC classification:
  • 617.69 21
Online resources: Available additional physical forms:
  • Issues also as CD.
Dissertation note: Thesis (M.Sc.)-Cairo University, 2021. Summary: The aim of the present study was to evaluate the marginal integrity of two types of ceramics; celtra duo and IPS Emax CAD vonlays restoring maxillary premolars. Methodology: A natural tooth represent first maxillary premolar was prepared according to regular dimensions of all ceramic restorations preparation guidelines, the prepared natural tooth was then duplicated into twenty epoxy resin dies, each duplicated epoxy die was scanned by 3 shape D500 extra oral scanner and then milled by Sirona MCX5 milling machine using IPS e.max CAD blocks and celtra duo CAD blocks. A total of twenty restorations were constructed, the samples were divided into two equal groups, ten samples for each group according to the material type used, group (I)ten vonlay samples (n=10) fabricated of IPS e.max CAD blocks, group (V) ten vonlays samples (n=10) fabricated of celtra duo CAD blocks. Marginal gap was measured using stereomicroscope. Result: It was found that Emax CAD vonlays recorded statistically non-significant higher marginal gap mean value (90.64µm ±9.64) than Celtra duo vonlays (88.46µm ±9.92). Conclusion: Both celtra duo and IPS e.max CAD have marginal integrity within the clinically acceptable range and can be safely used for premolar area. Summary: كان الهدف من هذه الرساله هو تقييم دقة حواف للضواحك المرممة بالقشور السطحية الخزفية المصنوعة من الليثيوم ديسليكات بالمقارنة مع القشور السطحية الخزفية المصنوعة من السيلتراديوالمصنعين بتكنولوجيا التصميم والخرط الحاسوبى التحكم. طبقا لعمليه حساب عدد العينات تم تصنيع عشرون عينة من القشور السطحية الخذفية و قسمت عشوائيا الي مجموعتين علي حسب نوع الماده (عشر عينات في كل مجموعه) : المجموعه الاولى : عشر عينات بتكنولوجيا التصميم و الخرط الحاسوبى التحكم من ماده الليثيوم دايسيليكات. المجموعه الثانيه : صنعت عشر عينات بتكنولوجيا التصميم و الخرط الحاسوبى التحكم من ماده السيلتراديو. تم تحضير ضاحك من الاسنان الطبيعية تمثل الضاحك الاول للفك العلوى طبقا للمعايير و القياسات المتفق عليها لتركيبات القشور الخزفية ثم تم عمل عشرون نسخه طبق الاصل من الضاحك الطبيعى باستخدام ماده راتنجات الايبوكسي بواسطه ماده السيلكون للمطابقه. تم عمل مسح ضوئي لكل نسخة من الضاحك المصنع من ماده راتنجات الايبوكسي المحضره باستخدام ماسح ضوئي من النوع المستخدم خارج الفم ثم تم عمل خرط العينات للمادتين المستخدمتين بواسطه ماكينه الخرط من النوع سيرونا ام سي اكس 5 باتباع التعليمات والطرق المنصوح بها من المصنع. تم تنظيف العينات ثم تم معالجة السطح المقابل للسنة باستخدام حمض الهٌدروفلورٌك و مادة السٌايلين، تم لصقهم بعد ذلك باستخدام مالط راتنجً ذاتً اللصق. اثناء اللصق تم الحفاظ علي العينات تحت الضغط المستمر باستخدام وزن ثابت ) ٢كغ( المثبت في جهاز التحميل المصمم خصيصا لتوحيد التحميل اثناء عملية اللصق. بعد ذلك تم قياس دقة الحواف لكل سطح لجمٌع القشور بعد اللزق بإستخدام المجهر الضوئي عند عامل تكبير 30 و من ثم تم جمع البيانات و جدولتها و تحليلها احصائيا للكشف عن اي قيم ذات اهمية بين المجموعتين بعد اختبار دقة الحواف.
Tags from this library: No tags from this library for this title. Log in to add tags.
Star ratings
    Average rating: 0.0 (0 votes)
Holdings
Item type Current library Home library Call number Status Barcode
Thesis Thesis قاعة الرسائل الجامعية - الدور الاول المكتبة المركزبة الجديدة - جامعة القاهرة Cai01.09.09.M.Sc.2021.Ho.E (Browse shelf(Opens below)) Not for loan 01010110087859000

Thesis (M.Sc.)-Cairo University, 2021.

Bibliography: pages 76-81.

The aim of the present study was to evaluate the marginal integrity of two types of ceramics; celtra duo and IPS Emax CAD vonlays restoring maxillary premolars.
Methodology: A natural tooth represent first maxillary premolar was prepared according to regular dimensions of all ceramic restorations preparation guidelines, the prepared natural tooth was then duplicated into twenty epoxy resin dies, each duplicated epoxy die was scanned by 3 shape D500 extra oral scanner and then milled by Sirona MCX5 milling machine using IPS e.max CAD blocks and celtra duo CAD blocks. A total of twenty restorations were constructed, the samples were divided into two equal groups, ten samples for each group according to the material type used, group (I)ten vonlay samples (n=10) fabricated of IPS e.max CAD blocks, group (V) ten vonlays samples (n=10) fabricated of celtra duo CAD blocks. Marginal gap was measured using stereomicroscope.
Result: It was found that Emax CAD vonlays recorded statistically non-significant higher marginal gap mean value (90.64µm ±9.64) than Celtra duo vonlays (88.46µm ±9.92).
Conclusion: Both celtra duo and IPS e.max CAD have marginal integrity within the clinically acceptable range and can be safely used for premolar area.

كان الهدف من هذه الرساله هو تقييم دقة حواف للضواحك المرممة بالقشور السطحية الخزفية المصنوعة من الليثيوم ديسليكات بالمقارنة مع القشور السطحية الخزفية المصنوعة من السيلتراديوالمصنعين بتكنولوجيا التصميم والخرط الحاسوبى التحكم.
طبقا لعمليه حساب عدد العينات تم تصنيع عشرون عينة من القشور السطحية الخذفية و قسمت عشوائيا الي مجموعتين علي حسب نوع الماده (عشر عينات في كل مجموعه) :
المجموعه الاولى : عشر عينات بتكنولوجيا التصميم و الخرط الحاسوبى التحكم من ماده الليثيوم دايسيليكات.
المجموعه الثانيه : صنعت عشر عينات بتكنولوجيا التصميم و الخرط الحاسوبى التحكم من ماده السيلتراديو.
تم تحضير ضاحك من الاسنان الطبيعية تمثل الضاحك الاول للفك العلوى طبقا للمعايير و القياسات المتفق عليها لتركيبات القشور الخزفية ثم تم عمل عشرون نسخه طبق الاصل من الضاحك الطبيعى باستخدام ماده راتنجات الايبوكسي بواسطه ماده السيلكون للمطابقه.
تم عمل مسح ضوئي لكل نسخة من الضاحك المصنع من ماده راتنجات الايبوكسي المحضره باستخدام ماسح ضوئي من النوع المستخدم خارج الفم ثم تم عمل خرط العينات للمادتين المستخدمتين بواسطه ماكينه الخرط من النوع سيرونا ام سي اكس 5 باتباع التعليمات والطرق المنصوح بها من المصنع.
تم تنظيف العينات ثم تم معالجة السطح المقابل للسنة باستخدام حمض الهٌدروفلورٌك و مادة السٌايلين، تم لصقهم بعد ذلك باستخدام مالط راتنجً ذاتً اللصق. اثناء اللصق تم الحفاظ علي العينات تحت الضغط المستمر باستخدام وزن ثابت ) ٢كغ( المثبت في جهاز التحميل المصمم خصيصا لتوحيد التحميل اثناء عملية اللصق.
بعد ذلك تم قياس دقة الحواف لكل سطح لجمٌع القشور بعد اللزق بإستخدام المجهر الضوئي عند عامل تكبير 30 و من ثم تم جمع البيانات و جدولتها و تحليلها احصائيا للكشف عن اي قيم ذات اهمية بين المجموعتين بعد اختبار دقة الحواف.