Optimization of some physical properties of nano-sized carbon black- loaded rubber blends / Ahmed Sabry Abdelrahman Thabet ; Supervised H. H. Hassan , S. S. Abdelaziz , M. H. M. Soleiman

By: Contributor(s): Material type: TextTextLanguage: English Publication details: Cairo : Ahmed Sabry Abdelrahman Thabet , 2016Description: 199 P. : charts , facsimiles ; 25cmOther title:
  • {uFE98}{uFECC}{uFEC5}{uFEF4}{uFEE1} {uFE8D}{uFEDF}{uFEA8}{uFEED}{uFE8D}{uFEB9} {uFE8D}{uFEDF}{uFED4}{uFEF4}{uFEAF}{uFEF4}{uFED8}{uFEF4}{uFE94} {uFEDF}{uFE98}{uFEED}{uFEDF}{uFEF4}{uFED4}{uFE8E}{uFE95} {uFE8D}{uFEDF}{uFEE4}{uFEC1}{uFE8E}{uFEC1} {uFE8D}{uFEDF}{uFEE4}{uFEA4}{uFEE4}ل {uئإ٩٢}{uئإإ٨}{uئإ٨إ}{uئإإ٨}{uئإإؤ}{uئإإ٨}{uئإئ٤}{uئإ٩٤} {uئإ٨٣}{uئإآ٤}{uئإإؤ}{uئإء٩} {uئإ٨ؤ}{uئإؤئ}{uئإؤأ}{uئإءؤ}{uئإ٩٢}{uئإإؤ}{uئإإ٥} [Added title page title]
Subject(s): Available additional physical forms:
  • Issued also as CD
Dissertation note: Thesis (Ph.D.) - Cairo University - Faculty of Science - Department of Physics Summary: The present work concerns with the optimization of some physical properties of rubber blends based on natural rubber (NR) and Styrene-Butadiene Rubber (SBR-1502). In addition two types of reinforcing nano-fillers; Intermediate Super Abrasion Furnace Black (ISAF N220) and Semi-Reinforcing Furnace Black (SRF N774) which have different physical and chemical properties are used. The object of this work was classified into three groups as follows: {uF0D8} Group one: To study the effect of NR content on the physico-mechanical, physico-chemical and electrical conductivity of NR/SBR rubber blends. {uF0D8} Group two: To study the effect of different concentrations of N220 and N774 blacks on the physico-mechanical, physico-chemical and electrical conductivity of the above vulcanizates. {uF0D8} Group three: To study the effect of the addition of mixed ratios of N220 and N774 nano-fillers on the physico-mechanical, physico-chemical and electrical conductivity. The order of addition of carbon black was also studied. It was found that, the optimum values of tensile strength and elongation at break are obtained for 50NR/50SBR rubber blends. The incorporation of this optimum blend with carbon black N220 and N774 enhance the mechanical properties and the optimum peak value for N220 black was detected at 40 phr while for N774 black at 60 phr. For mixed types of carbon black, there are no remarkable effect for the order of addition on the values of tensile strength and/or elongation at break, while it affect the mobility of charge carriers. The addition of N220 after the existence of N774 black exhibits higher mobility than the inverse order regardless of the N220/N774 ratio
Tags from this library: No tags from this library for this title. Log in to add tags.
Star ratings
    Average rating: 0.0 (0 votes)
Holdings
Item type Current library Home library Call number Copy number Status Date due Barcode
Thesis Thesis قاعة الرسائل الجامعية - الدور الاول المكتبة المركزبة الجديدة - جامعة القاهرة Cai01.12.20.Ph.D.2016.Ah.O (Browse shelf(Opens below)) Not for loan 01010110070140000
CD - Rom CD - Rom مخـــزن الرســائل الجـــامعية - البدروم المكتبة المركزبة الجديدة - جامعة القاهرة Cai01.12.20.Ph.D.2016.Ah.O (Browse shelf(Opens below)) 70140.CD Not for loan 01020110070140000

Thesis (Ph.D.) - Cairo University - Faculty of Science - Department of Physics

The present work concerns with the optimization of some physical properties of rubber blends based on natural rubber (NR) and Styrene-Butadiene Rubber (SBR-1502). In addition two types of reinforcing nano-fillers; Intermediate Super Abrasion Furnace Black (ISAF N220) and Semi-Reinforcing Furnace Black (SRF N774) which have different physical and chemical properties are used. The object of this work was classified into three groups as follows: {uF0D8} Group one: To study the effect of NR content on the physico-mechanical, physico-chemical and electrical conductivity of NR/SBR rubber blends. {uF0D8} Group two: To study the effect of different concentrations of N220 and N774 blacks on the physico-mechanical, physico-chemical and electrical conductivity of the above vulcanizates. {uF0D8} Group three: To study the effect of the addition of mixed ratios of N220 and N774 nano-fillers on the physico-mechanical, physico-chemical and electrical conductivity. The order of addition of carbon black was also studied. It was found that, the optimum values of tensile strength and elongation at break are obtained for 50NR/50SBR rubber blends. The incorporation of this optimum blend with carbon black N220 and N774 enhance the mechanical properties and the optimum peak value for N220 black was detected at 40 phr while for N774 black at 60 phr. For mixed types of carbon black, there are no remarkable effect for the order of addition on the values of tensile strength and/or elongation at break, while it affect the mobility of charge carriers. The addition of N220 after the existence of N774 black exhibits higher mobility than the inverse order regardless of the N220/N774 ratio