Micro-shear bond strength of conventional and self-adhesive flowable resin composites to resin-modified glass ionomer cement base material following different surface treatments : An in vitro study / Khaldoun Kazem Asaad Shawar ; Supervised Mostafa Abdulhameed Mostafa Hassan , Amir Hafez Ibrahim
Material type:
- قوه رابطه القص المجهريه للكومبوزيت الراتينجى التقليدى و المسال مع قاعده اسمنت الايونومر الزجاجى المعدل بالراتينج بعد معالجات السطح المختلفه : دراسه معمليه [Added title page title]
- Issued also as CD
Item type | Current library | Home library | Call number | Copy number | Status | Barcode | |
---|---|---|---|---|---|---|---|
![]() |
قاعة الرسائل الجامعية - الدور الاول | المكتبة المركزبة الجديدة - جامعة القاهرة | Cai01.09.03.M.Sc.2015.Kh.M (Browse shelf(Opens below)) | Not for loan | 01010110073687000 | ||
![]() |
مخـــزن الرســائل الجـــامعية - البدروم | المكتبة المركزبة الجديدة - جامعة القاهرة | Cai01.09.03.M.Sc.2015.Kh.M (Browse shelf(Opens below)) | 73687.CD | Not for loan | 01020110073687000 |
Browsing المكتبة المركزبة الجديدة - جامعة القاهرة shelves Close shelf browser (Hides shelf browser)
Thesis (M.Sc.) - Cairo University - Faculty of Oral and Dental Medicine - Department of Operative Dentistry
Objectives: The aim of this study was to evaluate and compare the effects of etching and adhesive application on the micro-shear bond strength of THREE types of resin composites; conventional packable nano composite, conventional flowable and self-adhesive flowable RC; to evaluate their bond strength with resin-modified glass ionomer base material after different surface treatments. Methods: A total number of 90 specimen were used in this study and divided randomly into three groups according to type of composite used and surface treatment applied the. RMGI discs were prepared using a cylindrical teflon mold. After light cure the teflon mold was removed around discs and placed inside clear acrylic mold, micro-cylinders of composite were constructed on the prepared surfaces using tygon tubes of 1 mm height and 0.7 mm internal diameter and The specimens were left in distilled water for 24 hour prior to the removal of tygon tube the tubes were then carefully cut using a lancet the micro-shear bond strength was determined in a universal testing machine. A Two way-ANOVA used to study the effect of different restorative materials and surface treatment of glass Ionomer on mean microshear bond test oSBS