header
Local cover image
Local cover image
Image from OpenLibrary

Effect of finish line steepness and construction technique on vertical marginal gap distance of machinable and pressable ips e-max ceramic copings : An in vitro study / Esraa Hashem Ahmed ; Supervised Ghada Ibrahim Shehab , Hanaa Ibrahem Sallam

By: Contributor(s): Material type: TextTextLanguage: English Publication details: Cairo : Esraa Hashem Ahmed , 2016Description: 117 P. : charts , facsimiles , photographs ; 25cmOther title:
  • فى التغطيات IPS E-MAX تأثير إنحدار خط النهاية و تقنية البناء على المسافة الرأسية الحافية الخزفية المميكنة و المضغوطة : دراسة معملية [Added title page title]
Subject(s): Online resources: Available additional physical forms:
  • Issued also as CD
Dissertation note: Thesis (M.Sc.) - Cairo University - Faculty of Oral and Dental Medicine - Department of Prosthodontics Summary: The aim of this in-vitro study was to assess the effect of finish line steepness (1 and 3 mm) and construction technique ( machinable and pressable ) on the vertical marginal gap distance of the IPS e.max ceramic copings In this study a total of 54 IPS e.max ceramic copings were constructed and divided according to construction technique into two main groups: Group I (n=14): Machinable all ceramic copings (IPS e.max CAD) Group II (n=40): Heat pressed all ceramic copings (IPS e.max Press) Each group was further subdivided into two subgroups according to different finish line steepness: Subgroup 1 : 1-mm finish line steepness Subgroup 2 : 3-mm finish line steepness Two ivory upper central incisors with same dimensions were selected, mounted in a stone base and prepared to receive full coverage all ceramic crowns with the two different finish line steepness using dental milling surveyor. Two nickel chromium dies with two different finish line steepnesses were then fabricated by duplication from the two prepared ivory upper central incisors. Machinable and pressable IPS e.max ceramic copings were constructed on these metal dies according to the manufacturer instruction following standardized protocol. For all samples, vertical marginal gap distance was measured at three selected points on the middle third of each surface of the die. The marginal area were photographed under magnification of x40 with digital camera attached to a stereomicroscope which was coupled to a computerized Quantitative analysis system, by means of software. The vertical marginal gap distance was measured in micrometers (æm). Each measurement was repeated three times, with all measurements being performed by a single investigator. Data were collected, tabulated and statistically analyzed
Tags from this library: No tags from this library for this title. Log in to add tags.
Star ratings
    Average rating: 0.0 (0 votes)
Holdings
Item type Current library Home library Call number Copy number Status Barcode
Thesis Thesis قاعة الرسائل الجامعية - الدور الاول المكتبة المركزبة الجديدة - جامعة القاهرة Cai01.09.09.M.Sc.2016.Es.E (Browse shelf(Opens below)) Not for loan 01010110074846000
CD - Rom CD - Rom مخـــزن الرســائل الجـــامعية - البدروم المكتبة المركزبة الجديدة - جامعة القاهرة Cai01.09.09.M.Sc.2016.Es.E (Browse shelf(Opens below)) 74846.CD Not for loan 01020110074846000

Thesis (M.Sc.) - Cairo University - Faculty of Oral and Dental Medicine - Department of Prosthodontics

The aim of this in-vitro study was to assess the effect of finish line steepness (1 and 3 mm) and construction technique ( machinable and pressable ) on the vertical marginal gap distance of the IPS e.max ceramic copings In this study a total of 54 IPS e.max ceramic copings were constructed and divided according to construction technique into two main groups: Group I (n=14): Machinable all ceramic copings (IPS e.max CAD) Group II (n=40): Heat pressed all ceramic copings (IPS e.max Press) Each group was further subdivided into two subgroups according to different finish line steepness: Subgroup 1 : 1-mm finish line steepness Subgroup 2 : 3-mm finish line steepness Two ivory upper central incisors with same dimensions were selected, mounted in a stone base and prepared to receive full coverage all ceramic crowns with the two different finish line steepness using dental milling surveyor. Two nickel chromium dies with two different finish line steepnesses were then fabricated by duplication from the two prepared ivory upper central incisors. Machinable and pressable IPS e.max ceramic copings were constructed on these metal dies according to the manufacturer instruction following standardized protocol. For all samples, vertical marginal gap distance was measured at three selected points on the middle third of each surface of the die. The marginal area were photographed under magnification of x40 with digital camera attached to a stereomicroscope which was coupled to a computerized Quantitative analysis system, by means of software. The vertical marginal gap distance was measured in micrometers (æm). Each measurement was repeated three times, with all measurements being performed by a single investigator. Data were collected, tabulated and statistically analyzed