Micro-shear bond strength of fluoride containing self-etch versus conventional self-etch adhesives on bond strength to dentin / Mohamed Ahmed Hashem ; Supervised Olfat Elsayed Hassanein , Mohamed Fouad Haridy
Material type:
- قوة الربط القصي الدقيقة باستخدام اللاصق ذاتي التخريش المحتوي على الفلورايد مقابل اللاصق ذاتي التخريش التقليدي علي قوة الربط للعاج السني : دراسة في المختبر [Added title page title]
- Issued also as CD
Item type | Current library | Home library | Call number | Copy number | Status | Barcode | |
---|---|---|---|---|---|---|---|
![]() |
قاعة الرسائل الجامعية - الدور الاول | المكتبة المركزبة الجديدة - جامعة القاهرة | Cai01.09.03.M.Sc.2017.Mo.M (Browse shelf(Opens below)) | Not for loan | 01010110075983000 | ||
![]() |
مخـــزن الرســائل الجـــامعية - البدروم | المكتبة المركزبة الجديدة - جامعة القاهرة | Cai01.09.03.M.Sc.2017.Mo.M (Browse shelf(Opens below)) | 75983.CD | Not for loan | 01020110075983000 |
Browsing المكتبة المركزبة الجديدة - جامعة القاهرة shelves Close shelf browser (Hides shelf browser)
Thesis (M.Sc.) - Cairo University - Faculty of Oral and Dental Medicine - Department of Operative Dentistry
This study was conducted to evaluate the effect of incorporating anti-cariogenic agent i.e. Fluoride, into self-etch adhesives on Micro-shear bond strength of resin composite to Dentin and to compare between Immediate and Delayed Micro-shear bond strength. The study compared two self-etch adhesive systems, one served as intervention (ClearFil liner bond F) and the other served as control (ClearFil s3 bond). Sixty-four extracted molars were collected, divided into four groups according to either fluoride-containing Immediate or non-fluoride containing Immediate and fluoride-containing Delayed or non-fluoride containing Delayed. The tested adhesive systems were applied to each specimen according to manufactures instructions where a polyethylene micro-tube were attached during bonding procedure, which later was packed with composite resin creating 4 micro-cylinders on the occlusal surface of each specimen. For evaluation of the micro-shear bond strength, prepared specimens where subjected to micro-shear stress using a universal testing machine and data was recorded for each specimen. To assess the ultra-morphological structure of the resin/dentin interface, Interfaces were analyzed under Environmental Scanning Electron Microscope at high magnifications.6 Conclusions Within the Limitations of this study, the following conclusions were possible: 1.The incorporation of Fluoride into self-etch adhesives was advantageous regarding immediate and delayed bond strength.2.Two-steps Self-etch adhesives system provided superior bonding capabilities compared to one step self-etch adhesives