TY - BOOK AU - Tamer Zui Hemma AU - Mona Ismail Riad , AU - Sahar Ahmed Abdelhalim , TI - Bond degradation resistance of nano - bond adhesive system bonded to dentin : : In vivo study / PY - 2011/// CY - Cairo : PB - Tamer Zui Hemma , KW - Bond degradation resistance KW - Dentin KW - Nano - bond adhesive system bonded N1 - Thesis (M.Sc.) - Cairo University - Faculty of Oral and Dental Medicine - Department of Opertive Dentistry; Issued also as CD N2 - This study was carried to evaluate the invivo bond degradation resistance of light and dual cure Nano Bond adhesive system by assessing the nanoleakage of class II resin composite restoration with and without etching, and interfacial analysis using ESEM and to investigate whether the curing mode and pre - etching could affect microtensile bond strength at 24 hours and after 3 monthes. Standardized class II cavities were prepared in 80 premolars of 20 patients. Dual and light cured Nano bond self etch adhesive was applied with and without pre - treatment. Then, teeth were extracted as part of orthodontic treatment according to testing periods. Sticks of 1mm2 cross section were prepared for testing both microtensile bond strength and nanoleakage evaluation. The results were presented as mean and SD values; repeated measures anova followed by Mann - whitney test were used to analyze the results ER -