000 | 02892cam a2200349 a 4500 | ||
---|---|---|---|
003 | EG-GiCUC | ||
005 | 20250223031503.0 | ||
008 | 160507s2015 ua o f m 000 0 eng d | ||
040 |
_aEG-GiCUC _beng _cEG-GiCUC |
||
041 | 0 | _aeng | |
049 | _aDeposite | ||
097 | _aM.Sc | ||
099 | _aCai01.09.03.M.Sc.2015.Ma.M | ||
100 | 0 | _aMahmoud Mohamed Sayed Ahmed | |
245 | 1 | 0 |
_aMicro - shear bond strength durability of dual cured adhesives to enamel and dentin / _cMahmoud Mohamed Sayed Ahmed ; Supervised Amira Farid Elzoghby , Aliaa Mohamed Mahmoud Elwakeel , Amir Hafez Ibrahim |
246 | 1 | 5 | _aإستمرارية قوة الربط القصى الدقى لللواصق ذات المعالجة المزدوجة على المينا و العاج |
260 |
_aCairo : _bMahmoud Mohamed Sayed Ahmed , _c2015 |
||
300 |
_a73 P. : _bphotographs ; _c25cm |
||
502 | _aThesis (M.Sc.) - Cairo University - Faculty of Oral and Dental Medicine - Department of Operative Dentistry | ||
520 | _aThe aim of this study was to evaluate and compare the micro - shear bond strength of two dual cure adhesive systems (futurabond DC and Futurabond U) versus one light cure adhesive system (solobond M) to enamel and dentin after storage for twenty four hours and one month. A total number of 120 teeth were used. The roots of each tooth were removed. For enamel specimens, cusps were ground up to 1 mm to produce flat surface using 600-grit silicon carbide paper under running water. While for dentin specimens, the occlusal enamel was removed and the dentin surface was ground flat until the distance between dentin surface and the highest pulp horn was 1 mm. Half of the specimens were stored in artificial saliva for 24 hours and the other half stored for one month then the microshear bond strength was determined in a universal testing machine. For enamel specimens, the 24 hrs period, futurabond U scored the highest value followed by solobond M then Futurabond DC with significant difference. Same as for 1 month period (but with decreased value) where futurabond U scored the highest value followed by solobond M then futurabond DC with significant difference. While for dentin specimens, the 24 hrs period, futurabond DC scored the highest value followed by futurabond U then solobond M with significant difference. Same as for 1 month period (but with decreased value) where futurabond DC scored the highest value followed by futurabond U then solobond M with significant difference | ||
530 | _aIssued also as CD | ||
653 | 4 | _aBonding agent | |
653 | 4 | _aDeep dentin | |
653 | 4 | _aDual cure | |
700 | 0 |
_aAliaa Mohamed Mahmoud Elwakeel , _eSupervisor |
|
700 | 0 |
_aAmir Hafez Ibrahim , _eSupervisor |
|
700 | 0 |
_aAmira Farid Elzoghby , _eSupervisor |
|
856 | _uhttp://172.23.153.220/th.pdf | ||
905 |
_aNazla _eRevisor |
||
905 |
_aSamia _eCataloger |
||
942 |
_2ddc _cTH |
||
999 |
_c56302 _d56302 |