000 | 02998cam a2200337 a 4500 | ||
---|---|---|---|
003 | EG-GiCUC | ||
005 | 20250223032033.0 | ||
008 | 180825s2017 ua dh f m 000 0 eng d | ||
040 |
_aEG-GiCUC _beng _cEG-GiCUC |
||
041 | 0 | _aeng | |
049 | _aDeposite | ||
097 | _aM.Sc | ||
099 | _aCai01.09.09.M.Sc.2017.En.E | ||
100 | 0 | _aEnas Alsayed Abedalazeem | |
245 | 1 | 0 |
_aEffect of long term storage and thermo-cycling on the vertical marginal gap distance and micro-leakage of CAD/CAM provisional restoration material in comparison to self-cured composite provisional restoration material : _bAn in-vitro study / _cEnas Alsayed Abedalazeem ; Supervised Ghada Ibrahim Khalil Shehab , Lamiaa Sayed Kheiralla |
246 | 1 | 5 |
_aتأثير ظروف التخزين طويل المدى و التدوير الحراري على الدقة الحافية الرأسية و التسرب الميكروني للمكعبات الاكريلية القابلة للخرط لصناعة التركيبات الاستعاضية المؤقتة مقارنة بمادة الكومبوزيت للتركيبات الاستعاضية المؤقتة : _bدراسة معملية |
260 |
_aCairo : _bEnas Alsayed Abedalazeem , _c2017 |
||
300 |
_a126 P. : _bcharts , facsimiles ; _c25cm |
||
502 | _aThesis (M.Sc.) - Cairo University - Faculty of Oral and Dental Medicine - Department of Prosthodontics | ||
520 | _aFabrication of provisional restorations is an important step toward achieving a successful prosthetic treatment. A provisional restoration is used to protect and sedate the pulp of prepared abutments, promote periodontal healing and health, replace missing teeth, prevent migration of abutments and provide esthetics. Provisional restorations also assist in the development of occlusal schemes and evaluation of phonetics. In addition, they protect abutments from microleakage and chemical injuries and stabilize compromised teeth. This study was designed to investigate, in vitro, the effect of long term storage and thermo-cycling on the vertical marginal gap distance and microleakage of machinable acrylic blocks for provisional restoration (VITA CAD-Temp) in comparison to self-cured bis-acrylic composite provisional restoration material (Protemp 4). A total of twenty four provisional crowns were constructed and divided according to provisional materials into two main groups: Group A: 12 Provisional crowns were constructed from machinable acrylic blocks (VITA CAD-Temp). Group B:12 Provisional crowns were constructed from self-cured bis-acrylic composite (Protemp 4 ). 116 | ||
530 | _aIssued also as CD | ||
653 | 4 | _aCAD/CAM | |
653 | 4 | _aLong term storage and thermo-cycling | |
653 | 4 | _aThe vertical marginal gap distance | |
700 | 0 |
_aGhada Ibrahim Khalil Shehab , _eSupervisor |
|
700 | 0 |
_aLamiaa Sayed Kheiralla , _eSupervisor |
|
856 | _uhttp://172.23.153.220/th.pdf | ||