245 | 1 | 0 |
_aEffect of the crystallization process on the marginal and internal gaps of partially crystallized versus fully crystallized zirconium reinforced lithium silicate CAD/CAM crowns : _bAn in-vitro study / _cAlaa Samir Fathy Elashkar ; Supervised Adel Mohamed Eltannir , Maha Ahmed Taymour |
246 | 1 | 5 |
_aاثر عملية التبلور على الثغرات الهامشية والداخلية في تيجان جزئية التبلور إزاء كاملة التبلور الليثيوم سيليكيت المعززة بالزركونيا CAD/CAM : _bدراسة معملية |
260 |
_aCairo : _bAlaa Samir Fathy Elashkar , _c2018 |
||
300 |
_a110 P. : _bcharts , photographs ; _c25cm |
||
502 | _aThesis (M.Sc.) - Cairo University - Faculty of Oral and Dental Medicine - Department of Prosthodontics | ||
520 | _aStatement of the problem: The precision of fit of chair-side CAD-CAM Zirconia reinforced lithium silicate crowns is still under research and the effect of post milling protocol on the marginal adaptation is not yet clearly stated in literature. Purpose: The aim of this study was to evaluate the marginal adaptation of fully crystallized versus partially crystallized zirconia reinforced lithium silicate (ZLS) ceramic computer-aided design/computer-aided manufacturing (CAD/CAM) fabricated crowns using stereomicroscope. Materials and methods: A total of 16 ceramic zirconia reinforced lithium silicate crowns. They were divided into two groups according to the degree of crystallization. The marginal adaptation of the fully crystallized zirconia reinforced lithium silicate CELTRA DUO (Dentsply, Sirona, Germany), were compared with the partially crystallized zirconia reinforced lithium silicate VITA SUPRINITY (VITA Zahnfabrik,Germany) after its crystallization. The 16 crowns (n=8 each group) were fabricated using a chair side CAD-CAM system. The crowns and die/crown assembly were viewed under stereomicroscope. 36 measurements were made for each crown, 9 measurements on each surface. The vertical marginal gap was directly viewed and measured using stereomicroscope. Data were recorded and statistically analyzed using the t- test and Two-way ANOVA test. The significance level was set at P {u2264} 0.05 | ||
530 | _aIssued also as CD | ||
653 | 4 | _aCeltra Duo | |
653 | 4 | _aMarginal adaptation | |
653 | 4 | _aVita Suprinity | |
700 | 0 |
_aAdel Mohamed Eltannir , _eSupervisor |
|
700 | 0 |
_aMaha Ahmed Taymour , _eSupervisor |
|
905 |
_aAsmaa _eCataloger |
||
905 |
_aNazla _eRevisor |
||
942 |
_2ddc _cTH |
||
999 |
_c74458 _d74458 |