100 0 _aBassima Edris Abdelhameed Mohammad
245 1 0 _aMarginal integrity of cemented hybrid ceramic(cerasmart) versus zirconia reinforced lithium disilicate ceramic (vita suprinity) occlusal veneers under cyclic loading :
_bIn-vitro study /
_cBassima Edris Abdelhameed Mohammad ; Supervised Lamiaa Sayed Kheiralla , Gihan Abdelhady Elnaggar
246 1 5 _aدقة حواف القشرة السطحية المصنعة من السيراميك المهجن (سيراسمارت) مقارنة بالليثيام ديسيليكات المقوى بالزركونيا (فيتا سوبرينيتى) الملصقة بعد التعرض للتحميل الدورى :
_bدراسة معملية
260 _aCairo :
_bBassima Edris Abdelhameed Mohammad ,
_c2018
300 _a87 P. :
_bcharts , photographs ;
_c25cm
502 _aThesis (M.Sc.) - Cairo University - Faculty of Oral and Dental Medicine - Department of Prosthodontics
520 _aAim of the Study:The aim of the present study was to compare the marginal integrity of occlusal veneers made from hybrid ceramic (Cerasmart) and zirconia reinforced lithium disilicate (Vita Suprinity ) under thermal cycling and cyclic loading. Materials and Methods: A standardized tooth preparation was applied to 34 human first maxillary molars using CNC machine with anatomical occlusal surface preparation with 1 mm ferrule and 1 mm deep chamfer finish line. All teeth were restored with occlusal veneers with 1.8 thickness at the cusp tip and 1.2 mm at the central groove ( CEREC AC CAD /CAM system) . Hybrid ceramic (Cerasmart) and zirconia reinforced lithium disilicate (Vita Suprinity ) were used to mill the restorations (n=17). The intaglio surfaces were HF-etched and silanated (Vita Suprinity) or airborne-particle abraded and silanated (Cersasmart). All restorations were adhesively luted with self adhesive resin cement (Rely X Unicem). All specimens were subjected to thermal cycling and cyclic loading for 25000 cycles simulate 2 months. A weight of 5Kg which is comparable to 50 N of chewing force was exerted with thermal aging between 5{u02DA} C and 55{u02DA} C. The marginal gap distance of the specimen was photographed using USB Digital microscope with a built-in camera connected with an IBM compatible personal computer using a fixed magnification of 45X. Shots of the margins were taken for each specimen. Then morphometric measurements were done for each shot [4 equidistant landmarks along the cervical circumference for each surface of the specimen (Mesial, buccal, distal, and lingual). Measurement at each point was repeated five times. Then the data obtained were collected, tabulated and then subjected to statistical analysis
530 _aIssued also as CD
653 4 _aCyclic loading
653 4 _aHybrid ceramic(cerasmart)
653 4 _aOcclusal veneers
700 0 _aGihan Abdelhady Elnaggar ,
_eSupervisor
700 0 _aLamiaa Sayed Kheiralla ,
_eSupervisor
856 _uhttp://172.23.153.220/th.pdf
905 _aAsmaa
_eCataloger
905 _aNazla
_eRevisor
942 _2ddc
_cTH
999 _c74635
_d74635