| 000 | 04344namaa22004211i 4500 | ||
|---|---|---|---|
| 003 | OSt | ||
| 005 | 20260226111909.0 | ||
| 008 | 250827s2024 ua a|||frm||| 000 0 eng d | ||
| 040 |
_aEG-GICUC _bara _cEG-GICUC _dEG-GICUC _erda |
||
| 041 | 0 |
_aara _bara _beng |
|
| 049 | _aإيداع | ||
| 082 | 0 | 4 | _a745.10288 |
| 092 |
_a745.10288 _221 |
||
| 097 | _aمــــاجستير | ||
| 099 | _aCai01.14.03.M.Sc.2024.مح.ت | ||
| 100 | 0 |
_a،محمود رفاعي عبد العاطى عبد الحميد _eإعداد. |
|
| 245 | 1 | 0 |
_aتقييم معدلات تلف عناصر الالباستر الزخرفيه المعمارية وطرق ترميمها وحمايتها تطبيقا على نموذج مختار / _cإعداد محمودرفاعي عبد العاطى عبد الحميد؛ إشراف أ.د / سيد محمد سيد حميدة، أ.د. احمد خلف احمد عبد العال. |
| 246 | 1 | 5 | _aEvaluation of the rates of damage of architecturaldecorative alabaster elements and methods of their restoration and protection, applied on selected model / |
| 264 | 0 | _c2024. | |
| 300 |
_a143 صفحة : _bإيضاحيات ؛ _c30 سم. + _eCD. |
||
| 336 |
_atext _2rda content |
||
| 337 |
_aUnmediated _2rdamedia |
||
| 338 |
_avolume _2rdacarrier |
||
| 502 | _aأطروحة (ماجستير)-جامعة القاهرة، 2024. | ||
| 504 | _aببليوجرافيا: صفحات 132-143. | ||
| 520 | _aيعتبرمسجد محمد على باشا اكبر مبنى اثرى استخدمت فية احجار الالباستر المصرى لذا فقد ركزت الدراسة على دراسة العوامل المختلفة المؤثرة على احجار الالباستر المصرى المستخدم كتكسيات داخلية وخارجية ومظاهر التلف الناتجة عن كل عامل من هذه العوامل. وأشارت نتائج الدراسه الى ان خصائصه الفزيائيه مثل متوسط الكثافه 2.70 جرام/سم3 , ومتوسط امتصاص الماء 0.017% , ومتوسط المسامية 0.10% , ومتوسط مقاومة الضغط 581.33 كيلو جرام/ سم2, ومتوسط مقاومه الشد 4.84 ميجا باسكال, ومتوسط الضغط البرازيلى 10.97 ميجا باسكال, كما تشير نتائج الدراسه الى ان هذه العناصر المعماريه تعاني من التلف الشديد بفعل العوامل الاستاتيكيه وخاصه هبوط التربه اسفل المسجد اثناء اعمال الحفر في قاعات قصر الناصر محمد بن قلوون | ||
| 520 | _aThe Mosque of Muhammad Ali Pasha is considered the largest archaeological building in which Egyptian alabaster stones were used. Therefore, the study focused on studying the different factors affecting the Egyptian alabaster stones used as internal and external cladding and the manifestations of damage resulting from each of these factors. The results of the study indicated that its physical properties such as average density 2.70 g/cm3, average water absorption 0.017%, average porosity 0.10%, average compressive strength 581.33 kg/cm2, average tensile strength 4.84 MPa, and average Brazilian pressure 10.97 MPa. The results of the study also indicate that these architectural elements suffer from severe damage due to static factors, especially the subsidence of the soil under the mosque during excavation works in the halls of the palace of Al-Nasir Muhammad bin Qalawun. | ||
| 530 | _aصدر أيضًا كقرص مدمج. | ||
| 546 | _aالنص بالعربية والملخص باللغة الإنجليزية والعربية. | ||
| 650 | 7 |
_aالصيانة والاصلاح _2qrmak |
|
| 653 | 0 |
_aالالباستر المصرى المياة _aالمياة الأرضية _aالأملاح |
|
| 700 | 0 |
_aسيد محمد سيد حميدة _eمشرف أطروحة. |
|
| 700 | 0 |
_aاحمد خلف احمد عبد العال _eمشرف أطروحة. |
|
| 900 |
_b24-11-2024 _cسيد محمد سيد حميدة _cاحمد خلف احمد عبد العال _dمحسن صالح _dمرفت حسن خليل _Uجامعة القاهرة _Fكلية الآثار _Dقسم ترميم وصيانة الآثار |
||
| 905 | _aSara | ||
| 942 |
_2ddc _cTH _e21 _n0 |
||
| 999 | _c178751 | ||