245 1 0 _aOne year clinical evaluation of e.max laminate veneers with and without using galla chinnesis as natural cross linking and remineralizing agent before bonding to teeth with amelogenesis imperfecta :
_bArandomized controlled clinical Trial /
_cMohammed Gamal Fahmy ; Supervised Jylan Fouad Elguindy , Amina Zaki , Heba Hamza
246 1 5 _aعام من التقييم الاكلينيكى للوجوه التجميليه المصنعه من السيراميك الزجاجى (ايماكس) باستخدم وبدون استخدام ماده الجالا تشينينش كعامل طبيعى لاعاده المعادن للاسنان التى تعانى خلل فى تكوين الميناء :
_bتجربه اكلينيكيه عشوائيه
260 _aCairo :
_bMohammed Gamal Fahmy ,
_c2018
300 _a95 P. :
_bphotographs ;
_c25cm
502 _aThesis (M.Sc.) - Cairo University - Faculty of Oral and Dental Medicine - Department of Prosthodontics
520 _aCeramic laminate veneers show a successful esthetic and functional long- term service for their perfect color match, marginal integrity and mechanical properties. The minimum-thickness, ceramic laminate veneers are a conservative and esthetic alternative to re-establish the form, shape and color of anterior teeth. Mechanical behavior and marginal integrity are the major factors that affect the long- term prognosis of any restorations. This clinical study was done to evaluate the marginal integrity and post- operative sensitivity for e.max CAD veneers bonded with or without using Galla chinensis before bond application. Twenty four ceramic laminate veneers were fabricated for anterior teeth. The patients were divided into two groups according to the bonding technique Group A (control group) e.max CAD laminate veneers bonded with conventional technique. Group B (intervention group) e.max CAD laminate veneers bonded after application of Galla chinensis. Standardized preparation with butt joint design and chamfer finish line located supra gingival were performed for all the teeth. The fabrication of the veneers was performed using CAD/CAM (Vhf S1) machine, with software (Exocad). The veneers surfaces were treated and silanated according to the manufacture instruction of each ceramic and enamel surfaces were etched where total etch adhesive protocol was obeyed using BISCO. Survival rate in terms of (marginal adaptation and post-operative sensitivity) for both groups were evaluated according to united states public health services (USPHS) criteria
530 _aIssued also as CD
653 4 _aCeramic laminate veneers
653 4 _aE.max CAD
653 4 _aGalla chinensis
700 0 _aAmina Zaki ,
_eSupervisor
700 0 _aHeba Hamza ,
_eSupervisor
700 0 _aJylan Fouad Elguindy ,
_eSupervisor
856 _uhttp://172.23.153.220/th.pdf
905 _aAsmaa
_eCataloger
905 _aNazla
_eRevisor
942 _2ddc
_cTH
999 _c73620
_d73620