Image from OpenLibrary

Behavior of strengthened reinforced concrete columns after exposure to elevated temperature / by Marina Alkess Kerllos Ibrahim ; Supervisors Prof. Dr. Mohamed El-said said Issa, Prof. Dr. Khaled Farouk Omar El-Kashif.

By: Contributor(s): Material type: TextLanguage: English Summary language: English, Arabic Producer: 2023Description: 209 pages : illustrations ; 30 cm. + CDContent type:
  • text
Media type:
  • Unmediated
Carrier type:
  • volume
Other title:
  • دراسة سلوك الأعمدة الخرسانية المسلحة المدعمة بعد تعرضها لدرجات الحرارة العالية [Added title page title]
Subject(s): DDC classification:
  • 624.183
Available additional physical forms:
  • Issues also as CD.
Dissertation note: Thesis (Ph.D)-Cairo University, 2025. Summary: In this research, different techniques of repair of fired R.C. columns are compared. These include Carbon Fiber Reinforced Polymers (CFRP) sheets, steel jackets, and R.C. jackets. The main variables were considered, the strengthening technique, fire duration, degree of temperature, concrete cover, concrete compressive strength and the column cross section. The experimental investigation includes testing of twelve columns. The experimental results showed that the three strengthening techniques used in this study significantly improved the ultimate load-carrying capacity. Increasing the elevated temperature duration, decreased the ultimate carrying capacity of the RC column when subjected to elevated temperatures. The concrete compressive strength of the columns decreased by approximately 20 % and 50 % at elevated temperatures of 400 °C and 600 °C, respectively. In addition, an increase in the temperature resulted in a reduction in the load capacity with` an increase in the axial displacement of the tested columns. The experimental results and the theoretical results showed a conservative difference of 5%. Summary: عند تعرض الأعمدة الخرسانية لدرجات حرارة مرتفعة أو النار، تبدأ قوتها في التدهور. لذلك، يجب تقوية أو إصلاح العمود التالف. في هذا البحث، يتم مقارنة ثلاث تقنيات مختلفة لتدعيم الأعمدة الخرسانية المسلحة التي تتعرض للحريق. عند زيادة زمن الحريق، تنخفض القدرة على تحمل الأعمدة المسلحة عند تعرضها لدرجات حرارة مرتفعة. وهكذا تنخفض قدرة الأعمدة على تحمل الحمل النهائي بنسبة تقدر بحوالي 20 %، و 50 % عند درجات حرارة مرتفعة قدرها 400و 600درجة مئوية على التوالي. أيضًا، أدى زيادة درجة الحرارة إلى انخفاض في قدرة التحمل مع زيادة الازاحة للأعمدة المختبرة. أظهرت النتائج المعملية والنتائج النظرية فرقًا طفيفا بنسبة 5٪.
Tags from this library: No tags from this library for this title. Log in to add tags.
Star ratings
    Average rating: 0.0 (0 votes)
Holdings
Item type Current library Home library Call number Status Barcode
Thesis قاعة الرسائل الجامعية - الدور الاول المكتبة المركزبة الجديدة - جامعة القاهرة Cai01.13.05.Ph.D.2025.Ma.B (Browse shelf(Opens below)) Not for loan 01010110092635000

Thesis (Ph.D)-Cairo University, 2025.

Bibliography: pages 206-209.

In this research, different techniques of repair of fired R.C. columns are compared. These
include Carbon Fiber Reinforced Polymers (CFRP) sheets, steel jackets, and R.C. jackets.
The main variables were considered, the strengthening technique, fire duration, degree of
temperature, concrete cover, concrete compressive strength and the column cross section.
The experimental investigation includes testing of twelve columns. The experimental
results showed that the three strengthening techniques used in this study significantly
improved the ultimate load-carrying capacity. Increasing the elevated temperature
duration, decreased the ultimate carrying capacity of the RC column when subjected to
elevated temperatures. The concrete compressive strength of the columns decreased by
approximately 20 % and 50 % at elevated temperatures of 400 °C and 600 °C,
respectively. In addition, an increase in the temperature resulted in a reduction in the load
capacity with` an increase in the axial displacement of the tested columns. The
experimental results and the theoretical results showed a conservative difference of 5%.

عند تعرض الأعمدة الخرسانية لدرجات حرارة مرتفعة أو النار، تبدأ قوتها في التدهور. لذلك، يجب تقوية أو إصلاح العمود التالف. في هذا البحث، يتم مقارنة ثلاث تقنيات مختلفة لتدعيم الأعمدة الخرسانية المسلحة التي تتعرض للحريق. عند زيادة زمن الحريق، تنخفض القدرة على تحمل الأعمدة المسلحة عند تعرضها لدرجات حرارة مرتفعة. وهكذا تنخفض قدرة الأعمدة على تحمل الحمل النهائي بنسبة تقدر بحوالي 20 %، و 50 % عند درجات حرارة مرتفعة قدرها 400و 600درجة مئوية على التوالي. أيضًا، أدى زيادة درجة الحرارة إلى انخفاض في قدرة التحمل مع زيادة الازاحة للأعمدة المختبرة. أظهرت النتائج المعملية والنتائج النظرية فرقًا طفيفا بنسبة 5٪.

Issues also as CD.

Text in English and abstract in Arabic & English.

There are no comments on this title.

to post a comment.
Share
Cairo University Libraries Portal Implemented & Customized by: Eng. M. Mohamady Contacts: new-lib@cl.cu.edu.eg | cnul@cl.cu.edu.eg
CUCL logo CNUL logo
© All rights reserved — Cairo University Libraries
CUCL logo
Implemented & Customized by: Eng. M. Mohamady Contact: new-lib@cl.cu.edu.eg © All rights reserved — New Central Library
CNUL logo
Implemented & Customized by: Eng. M. Mohamady Contact: cnul@cl.cu.edu.eg © All rights reserved — Cairo National University Library