Image from OpenLibrary

Properties of concrete incorporating recycled crushed clay Bricks as coarse and fine aggregates / by Ahmed Maged Ahmed Naiem AbdEl-Moaty ; Supervisors Prof. Dr. Hatem Hassan Ali Ibrahim, Prof. Dr. Mohamed Karam Hussein Ismail.

By: Contributor(s): Material type: TextLanguage: English Summary language: English, Arabic Producer: 2025Description: 81 pages : illustrations ; 30 cm. + CDContent type:
  • text
Media type:
  • Unmediated
Carrier type:
  • volume
Other title:
  • خصائص الخرسانة المحتوية على طوب طفلي معاد تدويره كركام كبير و صغير [Added title page title]
Subject(s): DDC classification:
  • 620.13605
Available additional physical forms:
  • Issues also as CD.
Dissertation note: Thesis (M.Sc)-Cairo University, 2025. Summary: This study investigates the mechanical properties and durability of concrete incorporating varying percentages of recycled crushed clay brick aggregates as replacements for both coarse and fine aggregates. A total of ten mixtures were developed, using recycled crushed clay brick aggregate at replacement levels of 0%, 25%, 50%, 75%, and 100% for each aggregate type. Key properties assessed included density, absorption, sorptivity, ultrasonic velocity, rebound hammer performance, compressive strength, splitting tensile strength, flexural strength, impact resistance, and abrasion resistance. All tests were conducted both before and after exposure to elevated temperatures (200, 400, 600, and 800 °C). The results indicated that clay bricks can be recycled to produce aggregates for developing concrete that is viable for structural and non- structural applications, contributing to the development of sustainable building materials. Summary: تتناول هذه الدراسة الخرسانة التي تحتوي على نسب مختلفة من ركام الطوب الطفلي المعاد تدويره كبدائل لكل من الركام الكبير والصغير. تم تطوير عشرة خلطات إجمالاً، مع استخدام الطوب الطفلي المعاد تدويره بمستويات استبدال بلغت 0%، 25%، 50%، 75%، و100% لكل نوع من الركام. تضمنت الخصائص التي تم تقييمها كل من الكثافة، الامتصاص، خاصية الامتصاص الشعري، سرعة الموجات فوق الصوتية، مطرقة الارتداد، مقاومة الضغط، مقاومة شد الانفلاق، مقاومة الانحناء، مقاومة الصدم، ومقاومة البري. أجريت جميع الاختبارات قبل وبعد التعرض لدرجات حرارة مرتفعة (200، 400، 600، و800 درجة مئوية). وأشارت النتائج إلى أن الطوب الطفلي يمكن إعادة تدويره لصناعة ركام لإنتاج خرسانات صالحة للتطبيقات الانشائية والغير انشائية، مما يسهم في تطوير مواد بناء مستدامة.
Tags from this library: No tags from this library for this title. Log in to add tags.
Star ratings
    Average rating: 0.0 (0 votes)
Holdings
Item type Current library Home library Call number Status Barcode
Thesis قاعة الرسائل الجامعية - الدور الاول المكتبة المركزبة الجديدة - جامعة القاهرة Cai01.13.05.M.Sc.2025.Ah.P (Browse shelf(Opens below)) Not for loan 01010110092965000

Thesis (M.Sc)-Cairo University, 2025.

Bibliography: pages 77-81.

This study investigates the mechanical properties and durability of concrete incorporating
varying percentages of recycled crushed clay brick aggregates as replacements for both coarse
and fine aggregates. A total of ten mixtures were developed, using recycled crushed clay brick
aggregate at replacement levels of 0%, 25%, 50%, 75%, and 100% for each aggregate type. Key
properties assessed included density, absorption, sorptivity, ultrasonic velocity, rebound hammer
performance, compressive strength, splitting tensile strength, flexural strength, impact
resistance, and abrasion resistance. All tests were conducted both before and after exposure to
elevated temperatures (200, 400, 600, and 800 °C). The results indicated that clay bricks can be
recycled to produce aggregates for developing concrete that is viable for structural and non-
structural applications, contributing to the development of sustainable building materials.

تتناول هذه الدراسة الخرسانة التي تحتوي على نسب مختلفة من ركام الطوب الطفلي المعاد تدويره كبدائل لكل من الركام الكبير والصغير. تم تطوير عشرة خلطات إجمالاً، مع استخدام الطوب الطفلي المعاد تدويره بمستويات استبدال بلغت 0%، 25%، 50%، 75%، و100% لكل نوع من الركام. تضمنت الخصائص التي تم تقييمها كل من الكثافة، الامتصاص، خاصية الامتصاص الشعري، سرعة الموجات فوق الصوتية، مطرقة الارتداد، مقاومة الضغط، مقاومة شد الانفلاق، مقاومة الانحناء، مقاومة الصدم، ومقاومة البري. أجريت جميع الاختبارات قبل وبعد التعرض لدرجات حرارة مرتفعة (200، 400، 600، و800 درجة مئوية). وأشارت النتائج إلى أن الطوب الطفلي يمكن إعادة تدويره لصناعة ركام لإنتاج خرسانات صالحة للتطبيقات الانشائية والغير انشائية، مما يسهم في تطوير مواد بناء مستدامة.

Issues also as CD.

Text in English and abstract in Arabic & English.

There are no comments on this title.

to post a comment.
Share
Cairo University Libraries Portal Implemented & Customized by: Eng. M. Mohamady Contacts: new-lib@cl.cu.edu.eg | cnul@cl.cu.edu.eg
CUCL logo CNUL logo
© All rights reserved — Cairo University Libraries
CUCL logo
Implemented & Customized by: Eng. M. Mohamady Contact: new-lib@cl.cu.edu.eg © All rights reserved — New Central Library
CNUL logo
Implemented & Customized by: Eng. M. Mohamady Contact: cnul@cl.cu.edu.eg © All rights reserved — Cairo National University Library